Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 6.04 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.04 GPa
876 ksi
ISO 178
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 50
Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin..
Flexural Modulus 6.04 GPa
876 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL FE1520PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1520PW resin is a blend of polyphenylene oxide (PPO) and polystyrene (PS) resin that contains 20% glass reinforcement. The resin is suitable for injection molding. Noryl FE1520PW resin has ..
Flexural Modulus 6.04 GPa
876 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PFB91S PA 6
LNP* THERMOCOMP* PFB91S is a compound based on Nylon 6 resin containing Proprietary Filler(s).
Flexural Modulus 6.04 GPa
876 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP PFB91S PA 6
LNP* THERMOCOMP* PFB91S is a compound based on Nylon 6 resin containing Proprietary Filler(s).