Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.02 GPa | 873 ksi | ASTM D790 |
Omni Plastics OmniTech™ ABS GR20 UV FD BK118, GY695 Flame Retardant UL Approved MaterialOmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, .. |
|||
Flexural Modulus | 6.02 GPa | 873 ksi | ASTM D790 |
Omni Plastics OmniTech™ ABS GRC20 NA Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Flexural Modulus | 6.02 GPa | 873 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |