Mechanical Properties Metric English Comments
Flexural Modulus 3.99 GPa
579 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS
PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications.
Flexural Modulus 3.99 GPa
579 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific)
10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors.
Flexural Modulus 3.99 GPa
579 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP KB006 Acetal
LNP* THERMOCOMP* KB006 is a compound based on Acetal containing 30% Glass Bead.
Flexural Modulus 3.99 GPa
579 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp DF002L PC (Asia Pacific)
LNP* THERMOCOMP* DF002L is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC-IP for the Asia P..
Flexural Modulus 3.99 GPa
579 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors.
Flexural Modulus 3.99 GPa
579 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFP32 PC
LNP* LUBRICOMP* DFP32 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.