Polymer Property : Flexural Modulus = 570.009 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.93001 - 113 GPa

@Temperature 65.6 - 177 °C
570.009 - 16400 ksi

@Temperature 150 - 350 °F
Average value: 32.8 GPa Grade Count:2
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..