Mechanical Properties Metric English Comments
Flexural Modulus 3.897 GPa
565.1 ksi
ASTM D790
Lucent Polymers GPCB-110 Polycarbonate+PBT, 10% Glass Fiber Reinforced
Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc.