Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.385 GPa @Temperature 120 °C |
55.8 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8202C HS PA6 (Dry) Ultramid 8202C HS is a heat stabilized, low viscosity, PA6 injection molding homopolymer possessing a modified crystalline structure for increased property performance and faster cycles. It is also.. |
|||
Flexural Modulus | 0.385 GPa @Temperature 120 °C |
55.8 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8202C PA6 (Dry) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Flexural Modulus | 0.385 GPa @Temperature 120 °C |
55.8 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8202CQ PA6 (Dry) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |