Mechanical Properties Metric English Comments
Flexural Modulus 3.77 GPa
547 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycolac® INP563 ABS
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
Flexural Modulus 3.77 GPa
547 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycolac® INP563 ABS+SAN
SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..