Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.7278 GPa | 540.67 ksi | ASTM D790 |
E-Polymers TEKAFIN® PH50GM 30% Glass Fiber Reinforced Mineral Filled Low Warpage Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |