Polymer Property : Flexural Modulus = 54.4 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.375 GPa
54.4 ksi
ASTM D 790
NOVA Chemicals Sclair® 72A Butene Copolymer LLDPE Injection Molding Resin
72A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. 72A is su..
Flexural Modulus 0.375 GPa

@Temperature 65.0 °C
54.4 ksi

@Temperature 149 °F
ASTM Test
BASF Ultramid® HPN 9350 HS PA6 (Dry)
Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res..