Polymer Property : Flexural Modulus = 526.1 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.627 GPa
526.1 ksi
ASTM D790
SABIC PS 155 General Purpose Polystyrene for Foam Extrusion
Product Description: General purpose Polystyrene PS 155 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with medium flow and go..
Flexural Modulus 3.627 GPa
526.1 ksi
ASTM D790
SABIC PS 160 General Purpose Polystyrene for Foam Extrusion
Product Description: General purpose Polystyrene PS 160 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle material having High molecular ..