Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 524.6 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.617 GPa
524.6 ksi
ASTM D790
Diamond Polymers SAN 250 with Lube Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Copyright © lookpolymers.com All Rights Reserved