Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.586 GPa | 520.1 ksi | ASTM D790 |
Lucent Polymers TPP-140 Polypropylene, Homopolymer, 40% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |