Polymer Property : Flexural Modulus = 5110 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 35.2 GPa
5110 ksi
Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite
Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwid..
Flexural Modulus 35.2 GPa
5110 ksi
Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite
Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwide..
Flexural Modulus 35.2 GPa
5110 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP LC008EXQ PEEK
LNP* THERMOCOMP* LC008EXQ is a compound based on Polyetheretherketone containing 40% Carbon Fiber. Added features of this grade include: Electrically Conductive, Easy Molding.