Polymer Property : Flexural Modulus = 5.96 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.96 GPa
864 ksi
ASTM D790
PolyOne Stat-Tech™ PI-05CF/000R Black Polyether Imide (PEI)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Modulus 5.96 GPa
864 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA
GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves.
Flexural Modulus 5.96 GPa
864 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA (Asia Pacific)
GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves.
Flexural Modulus 5.96 GPa
865 ksi
ASTM D790
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 IM10 Glass Reinforced/Impact Modified Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics