Flexural Modulus 5.67 GPa
822 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT
LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage.
Flexural Modulus 5.67 GPa
822 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Flexural Modulus 5.67 GPa
822 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.
Flexural Modulus 5.67 GPa
822 ksi
ASTM D790
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Asia Pacific)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.