Polymer Property : Flexural Modulus = 5.63 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.63 GPa
817 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6
LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity.
Flexural Modulus 5.63 GPa
817 ksi
Procedure B, Test Method I(chs 0.05 in/min); ASTM D790
Diamond Polymers ABS 3501 GF-30
Description: Reinforced Grade, 30%Glass FilledInformation provided by Diamond Polymers, Inc.