Polymer Property : Flexural Modulus = 5.43 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.43 GPa
788 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific)
Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications.