Mechanical Properties Metric English Comments
Flexural Modulus 5.394 GPa
782.3 ksi
ASTM D790
Kolon KOPET® KP133G15BL G/F Reinforced Polyester Compound Resin (PET)
Dimensionally stable, high elastic, high flowApplications: Ink CartridgeInformation provided by API-Kolon.
Flexural Modulus 5.394 GPa
782.3 ksi
ASTM D790
Kolon SPESIN® KP213G15BL Glass Fiber Reinforced PBT Compound Resin
b>Characteristics: G/F 15% reinforced, BLACKApplications: Impeller housingsInformation provided by API-Kolon.
Flexural Modulus 5.394 GPa
782.3 ksi
ASTM D790
Kolon SPESIN® KP213G15SIBL Glass Fiber Reinforced PBT Compound Resin
G/F 15%, high toughness, excellent surfaceApplications: Various types of housingsInformation provided by API-Kolon.