Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0360 GPa | 5.22 ksi | 1% Secant Modulus; ASTM D790 |
DSM Biomedical Elasthane™ 80A Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |