Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0359 GPa | 5.20 ksi | ASTM D790 |
Multibase Multi-Flex® A 7101 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |