Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.992845 - 5.19865 GPa @Temperature -40.0 - 121 °C |
144.002 - 754.012 ksi @Temperature -40.0 - 250 °F |
Average value: 2.30 GPa Grade Count:3 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |