Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.172 GPa | 750.1 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Flexural Modulus | 5.172 GPa | 750.1 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylex® P1010G20 HB Polycarbonate, 20% Fiberglass Reinforced Information provided by Ravago. |
|||
Flexural Modulus | 5.172 GPa | 750.1 ksi | Method 1, Proc. B; ASTM D-790-95 |
Multibase Multi-ABS 7522 R , 22% Filler Content Data provided by Multibase. |