Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.14 GPa | 745 ksi | Tangent; ASTM D790 |
RheTech Products GC30P101-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayFan shroudInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.14 GPa | 745 ksi | Tangent; ASTM D790 |
RheTech Products GC30P103-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Battery traysFender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.14 GPa | 745 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6 LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity. |
|||
Flexural Modulus | 5.14 GPa | 745 ksi | Tangent; ASTM D790 |
RheTech Products GC30P100-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Arm rest insertBattery trayBracketsAir cleaner housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.14 GPa | 745 ksi | Tangent; ASTM D790 |
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |