Mechanical Properties Metric English Comments
Flexural Modulus 5.04 GPa
731 ksi
ISO 178
SABIC Innovative Plastics LNP Lubricomp KFI12A Acetal Homopolymer
LNP LUBRICOMP* KFI12A is a compound based on Acetal Homopolymer resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABI..
Flexural Modulus 5.04 GPa
731 ksi
XY; ASTM D790
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer
This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire..