Polymer Property : Flexural Modulus = 497.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.432 GPa
497.8 ksi
Tangent, chs 0.05 in/min; ASTM D790
Network Polymers SAN 280 Water Clear
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Flexural Modulus 3.432 GPa
497.8 ksi
ASTM D790
Daelim H&L Plavis-C CM Conductive Polyimide Bearing
Compression Molded. Plavis-C: Conductive, Electrical conductive, high thermal resistance and superior mechanical properties. Surface resistivity 10²-10³ OhmGeneral Plavis information for all grad..
Flexural Modulus 3.432 GPa
497.8 ksi
ASTM D790
Daelim H&L Plavis-ESD CM Polyimide Bearing
Compression Molded. Plavis-ESD: Electrostatic dissipative, Electrostatic dissipative, high thermal resistance and superior mechanical properties. And surface resistivity 10²-10³ OhmGeneral Plavis..