Mechanical Properties Metric English Comments
Flexural Modulus 0.343 GPa
49.8 ksi
Zylog Hipolyene® 1703 MS HF Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 0.343 GPa
49.8 ksi
Zylog Hipolyene® 2703 MS EX 3 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 0.343 GPa
49.8 ksi
Zylog Hipolyene® 2703 MS Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 0.343 GPa

@Thickness 6.40 mm
49.8 ksi

@Thickness 0.252 in
15mm/min; ASTM D790
LG Chemical KEYFLEX BT S5035 Ester Type TPE
Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide..