Mechanical Properties Metric English Comments
Flexural Modulus 3.33 GPa
483 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion 87768 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 3.33 GPa
483 ksi
ASTM D790
Omni Plastics OmniTech™ PA6/6,6 V0 125 Flame Retardant
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Flexural Modulus 3.33 GPa
483 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP IFL21 PA 6/12 (Asia Pacific)
LNP* LUBRICOMP* IFL21 is a compound based on Nylon 6/12 resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.
Flexural Modulus 3.33 GPa
483 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM AUT210 PEI
Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti..
Flexural Modulus 3.33 GPa
483 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..
Flexural Modulus 3.33 GPa
483 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East)
Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o..