Polymer Property : Flexural Modulus = 462.4 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.188 GPa
462.4 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Nemcon™ H ABS DP116P ABS
ABS-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers