Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.58 - 3.16 GPa | 229 - 458 ksi | Average value: 2.44 GPa Grade Count:11 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |