Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 31.3 GPa
4540 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI
LNP* THERMOCOMP* EC008APQ is a compound based on Polyetherimide containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, High Flow.