Mechanical Properties Metric English Comments
Flexural Modulus 0.262 - 0.310 GPa
38.0 - 45.0 ksi
ASTM D790
Buckeye Polymers BP FLEX D4107 C BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..