Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 30.3 GPa | 4400 ksi | ASTM D790 |
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |