Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.3097 GPa @Temperature 23.0 °C |
44.92 ksi @Temperature 73.4 °F |
ASTM D790 |
Lubrizol Estane® 58144 Thermoplastic Polyurethane Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer.. |