Mechanical Properties Metric English Comments
Flexural Modulus 44.7 GPa
6480 ksi
ASTM D790
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
AMC™ 8593 NT is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high he..