Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 28.97 GPa | 4202 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp OC008A PPS - Branched LNP* Thermocomp* OC008A is a compound based on Branched Polyphenylene Sulfide containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |