Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.290 GPa | 42.0 ksi | ASTM D 790 |
Teknor Apex APEX® 02-A0310A-107 Polyvinyl Chloride, Semi-Rigid Notes: 80°C Insulation; RoHS Compliant Uses: Automotive Electronics; InsulationWire Types: GPTAgency Ratings: SAE J1128 Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor .. |
|||
Flexural Modulus | 0.290 GPa | 42.0 ksi | ASTM D790 |
Aaron Industries AAROLENE® ARPE LD 300-1 Low Density Polyethylene Compounded Resin AAROLENE® ARPE 300 Series Polyethylene Compounded Resin LDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified. |