Mechanical Properties Metric English Comments
Flexural Modulus 28.83 GPa
4181 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA
LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.