Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.87 GPa | 706 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.87 GPa | 706 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.87 GPa | 706 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.87 GPa | 706 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.87 GPa | 706 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.87 GPa | 706 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |