Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.799 GPa | 696.1 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334G25M5CL Glass/Mineral Reinforced Coupled |
|||
Flexural Modulus | 4.799 GPa | 696.1 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336G20M10CL Glass/Mineral Reinforced Coupled |
|||
Flexural Modulus | 4.799 GPa | 696.1 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339G25M5CL Glass/Mineral Reinforced Coupled |
|||
Flexural Modulus | 4.799 GPa | 696.1 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0339M40CL Mica Reinforced Coupled |