Polymer Property : Flexural Modulus = 4.79 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.79 GPa
695 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6
LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.