Mechanical Properties Metric English Comments
Flexural Modulus 4.66 GPa
676 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp WB008 PBT
LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region.