Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.43 GPa | 643 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RFI12 PA 66 LNP* LUBRICOMP* RFI12 is a compound based on Nylon 66 resin containing 10% Glass Fiber, 2% Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 4.43 GPa | 642 ksi | Procedure B, Test Method I(chs 0.05 in/min); ASTM D790 |
Diamond Polymers ABS 3501 GF-20 Description: Reinforced Grade, 20%Glass FilledInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 4.43 GPa | 643 ksi | ASTM D790 |
Clariant Renol BR7039G15 Nylon 6, 15% Glass Fiber, bondable to TPU Data provided by Clariant Masterbatches |