Mechanical Properties Metric English Comments
Flexural Modulus 4.231 GPa
613.7 ksi
ASTM D790
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black
DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman.
Flexural Modulus 4.231 GPa
613.7 ksi
ASTM D790
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black
DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman.
Flexural Modulus 4.231 GPa
613.7 ksi
ASTM D790
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black
DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman.
Flexural Modulus 4.231 GPa
613.7 ksi
ASTM D790
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black
DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman.
Flexural Modulus 4.231 GPa
613.7 ksi
ASTM D790
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black
DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman.
Flexural Modulus 4.231 GPa
613.7 ksi
ASTM D790
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black
DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman.