Mechanical Properties Metric English Comments
Flexural Modulus 0.0279 GPa
4.05 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE A 7020 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.