Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.50 - 4.00 GPa @Temperature 60.0 - 90.0 °C |
218 - 580 ksi @Temperature 140 - 194 °F |
Average value: 2.84 GPa Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Flexural Modulus | 1.70 - 4.00 GPa | 247 - 580 ksi | Average value: 2.37 GPa Grade Count:28 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |