Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 27.23 GPa | 3949 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |