Mechanical Properties Metric English Comments
Flexural Modulus 26.3 GPa
3810 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ECL36XXQ PEI
LNP* Lubricomp* ECL36XXQ is a compound based on Polyetherimide containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 26.3 GPa
3810 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EC006APQ PEI
LNP* Thermocomp EC006APQ is a compound based on Polyetherimide containing 30% Carbon Fiber. Added features include: Electrically Conductive, High Flow.