Polymer Property : Flexural Modulus = 379.4 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.616 GPa
379.4 ksi
ASTM D790
KEP Kepital® F40 Standard Grade/Low Viscosity Acetal Homopolymer
injection molding: electrical parts, machine/mechanical parts, industrial parts, automotive applications, electronic data processing.Kepital® is a registered trademark of Korea Engineering Plasti..