Mechanical Properties Metric English Comments
Flexural Modulus 2.599 GPa
377.0 ksi
(50.8 mm Span) 1mm/min; ASTM D790
LNP ULTEM® SMU6303 Polyetherimide, 5% Glass Fiber Reinforcement, 5% PTFE Lubricant  (discontinued **)
Will be UNTW05.Features: Lubricated, High Heat Resistance, Good Wear Resistance, Low to None Ion Content, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provide..