Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.587 GPa | 375.2 ksi | ASTM D790 |
Ineos Nova 5800 High Impact Polystyrene
(discontinued **) Balance of toughness and rigidity, Good gloss, USP Class VIApplications: Thermoformed and molded packaging, Drink cups and lids, Structural foam, Custom sheetProperties were determined on injection .. |